EXTERIOR PAINTING
147

gummy, sticky mass of paint is the result. This soon gums the knife, also forms a cement over the wood, which is very hard to remove. This is especially true where excessive painting has been done, the paint having been mixed with boiled oil or an excess of japan added, or where the paint has cracked when first applied and paint heavily applied over it in an attempt to fill the cracks, leaving the surface with an excess of oil paint spread over it.

If it is not possible to burn the paint off, it can be painted with fairly good results if first cleaned with a wire brush, breaking the edges of the paint that may have commenced to show signs of peeling and turning out, also removing all the dirt from the cracks, then applying a coat of paint mixed with from a pint to a quart of turpentine to the gallon of paint, according to the elasticity of the surface. Do not apply a heavier coat than is absolutely necessary. Be particular to brush the paint well. Do not have the paint too flat on the protected or more elastic portions of the building, as these parts are very easily affected by hot or humid weather. Do not attempt to rush the work. Allow ample time for the paint to harden, then apply a finishing coat of paint mixed to a good consistency reduced with 1-32 to 1-16 gallon turpentine to a gallon of paint. Brush out well. This will not blister nor pull the undercoats and will make a fairly satisfactory job.

Peeled Paint. In preparing the surface for the repainting of peeled work, the same care should be exercised as with cracked paint. Where the paint has commenced to peel in small chips and upon examination it is found that the trouble is with the last or finishing coat, such is called chipping or fluffing. The trouble can usually be traced to the improper application of the paint or its having been applied over dampness caused by dews or frosts, also the paint becoming chilled or applied in freezing weather, not allowing sufficient penetration, which caused it to soon chip or fluff off. This trouble can very easily be overcome by